In the front, Xiaobian has analyzed the woodworking composite process in the glue system solution for wooden doors, and today, I will share the solution of the veneer veneer process for wooden doors with glue! First of all, let's learn about the bark ~
Veneer, also known as thin wood, veneer, it is used in furniture and other products veneer decoration, is a kind of wood flake thin veneer or veneer material with precious tree species characteristics.
A long history: the earliest use of wood bark was found in Egypt 4000 years ago, due to the local tropical desert area, wood resources are tight, but the ruling class and the love and pursuit of precious wood, in this case, people invented the wood cutting.
Application field:
Veneer, as a kind of decorative wood products, has been applied in various fields:
1. Veneer is widely used in classical furniture, modern panel furniture, solid wood composite door surface veneer;
2. Wood bark is widely used in hotels, guesthouses, restaurants, cafes, entertainment clubs, townhouses and other interior decoration decoration surface;
3. Veneer is widely used in the interior decoration of cars and luxury yachts;
4. Veneer is widely used in piano, violin, high-end audio functional Musical Instruments, other wood products, handicrafts surface veneer.
technology
Wood veneer
With the rise of decorative heat, wood-based panels have become an indispensable role, and wood veneer, as a natural decorative material, gives the wood-based panels a beautiful natural pattern. The thickness of solid wood skin is generally between 0.1mm-0.6mm, and the thickness of wood skin should not be too thin, otherwise it is easy to produce permeation and infiltration in the process of processing.
The common use of veneer is to press veneer onto a wood-based board or fingerboard to create veneer panels, and then process them into furniture.
Manual veneer steps:
1. Wet the bark completely
2. Polish the surface of the object and apply glue
3. Put the veneer on the object to be attached, smooth it in a good position, and then gently scrape it with a scraper
4. Wait for the veneer and glue to dry, iron the veneer with an iron, and make it completely attached to the surface of the bottom layer
5. Use a sharp blade to cut off the excess wood along the sides
Frequently asked Questions
Pain Point 1
Veneer blistering is difficult to repair
Cause analysis
In the process of pasting, we often encounter a problem: that is, the hand-pasted veneer is easy to blister, and then the problem is that the veneer cracks after ironing. This problem has been plaguing many workers on the practical front line.
The reason for the foaming of wood bark, roughly speaking, there are the following situations in the operation:
1. Uneven bottom, that is, the density board substrate is not polished in place.
2. The glue problem, the use of non-standard glue, resulting in insufficient adhesive force, or the glue is not uniform enough.
3. The bark used is too thick and the bark is not wet at the same time.
4. The temperature of the iron is not well controlled, and the general temperature is too low and easy to bubble.